Grades We Manufacture

::
 

Grades Manufactured

ASTM STANDARDS

Carbon Steel ASTM A216 Gr. WCB, WCC
Alloy Steel ASTM A217 Gr. WC6, WC9, C12, C12A
Martensitic Stainless Steel ASTM A217 Gr. CA15, CA15M, SS410, Ss420
ASTM A352 Gr. CA6NM
Stainless Steel ASTM A351 Gr. CF3, CF3M, CF8, CF8M, CG8M, CF8C, CD4MCu, CN7M, CK3MCuN(6MO)
Precipitation Hardening Steel ASTM A747 Gr. CB7Cu1 / 17-4PH
Heat Resistant Steel ASTM A297 Gr. HE, HH, HK
Nickel Based Alloy Steel ASTM A494 Gr. M25S, M35-1, Cz100, Cy40
CW12 MW (HAC), CU5MCuC(INCONEL 825)
Cw6 MC(INCONEL 625), INCONEL 718
Duplex Steel &
Super Duplex Steel
ASTM A890/A995 Gr. 3A, 4A, 5A
ASTM A995 Gr. CD3MWCuN / 6A
Carbon Steel for
Low Temp. Service
ASTM A352 Gr. LCB, LCC, LC1, LC3 & 1C

DIN STANDARDS

EN 10213 1.0619
1.4308
1.4408
1.6220
1.7357
1.7379
1.4470
1.0625